bioRxiv Science⌕ Search

bioRxiv · 10.1101/2021.07.29.454385

3D printed cobalt-chromium-molybdenum porous superalloy with superior antiviral activity

Abstract

COVID-19 pandemic and associated supply-chain disruptions emphasise the requirement for antimicrobial materials for on-demand manufacturing. Besides aerosol transmission, SARS-CoV-2 is also propagated through contact with virus-contaminated surfaces. As such, the development of effective biofunctional materials that can inactivate SARS-CoV-2 are critical for pandemic preparedness. Such materials will enable the rational development of antiviral devices with prolonged serviceability reducing the environmental burden of disposable alternatives. This research reveals the novel use of Laser Powder Bed Fusion (LPBF) to 3D print porous Cobalt-Chromium-Molybdenum (Co-Cr-Mo) superalloy with potent antiviral activity (100% viral inactivation in 30 mins). The porous material was rationally conceived using a multi-objective surrogate model featuring track thickness (tt) and pore diameter ({phi}d) as responses. The regression analysis found the most significant parameters for Co-Cr-Mo track formation to be the interaction effects of scanning rate (Vs) and laser power (Pl) in the order PlVs > Vs > Pl. Contrastively, the pore diameter was found to be primarily driven by the hatch spacing (Sh). The study is the first to demonstrate the superior antiviral properties of 3D printed Co-Cr-Mo superalloy against an enveloped virus used as biosafe viral model of SARS-CoV-2. The material significantly outperforms the viral inactivation time of other broadly used antiviral metals such as copper and silver from 5 hours to 30 minutes. As such the study goes beyond the current state-of-the-art in antiviral alloys to provide extra-protection to combat the SARS-COV-2 viral spread. The evolving nature of the COVID-19 pandemic brings new and unpredictable challenges where on-demand 3D printing of antiviral materials can achieve rapid solutions while reducing the environmental impact of disposable devices. Graphical abstract O_FIG O_LINKSMALLFIG WIDTH=200 HEIGHT=148 SRC="FIGDIR/small/454385v1_ufig1.gif" ALT="Figure 1"> View larger version (47K): org.highwire.dtl.DTLVardef@992f2forg.highwire.dtl.DTLVardef@e8dbe5org.highwire.dtl.DTLVardef@1bcb8adorg.highwire.dtl.DTLVardef@100a345_HPS_FORMAT_FIGEXP M_FIG C_FIG

Source connections

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Arjunan, A., Robinson, J., Baroutaji, A., Marti, M., Tunon-Molina, A., Serrano-Aroca, A.. 2021-07-30. 3D printed cobalt-chromium-molybdenum porous superalloy with superior antiviral activity. https://doi.org/10.1101/2021.07.29.454385

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related preprints

Comparative study of chlorophyll measurement in Physcomitrium patens moss using a conventional microscope adapted for combined 2D+1D imaging and spectral analysis

Imaging spectroscopy often requires expensive and complex equipment. Here we show a simple procedure for attaching a standard miniature fiber spectrometer to a conventional microscope, allowing easy integration of 2D imaging with 1D high-resolution spectral measurements. This combination provides much of the benefit of a full imaging spectrometer without the large equipment investment, and we provide instructions for modifying microscopes to this setup and the present measurements of living cells that demonstrate their performance. Using this setup, we compare the quantitative measurement of chlorophyll concentration in Physcomitrium patens moss using color imaging and spectral sampling.

bioengineering↗

De novo designed single-domain antibodies protect against lethal cobra venom neurotoxicity in vivo

Generative protein design can now rapidly produce de novo binders with high affinity and functional activity against a wide range of targets, including lethal snake venom toxins. However, so far most reported successes rely on new-to-nature scaffolds with limited therapeutic precedent. Single-domain antibodies (VHHs) offer a clinically validated alternative scaffold that can bind and neutralize long-chain -neurotoxins, which are some of the most lethal components in snake venoms. Here we compare three recently established de novo design models with VHH-design capabilities (Germinal, RFantibody, and BoltzGen) for their ability to generate VHHs against the neurotoxin -cobratoxin from the monocled cobra (Naja kaouthia). Using standardized model inputs and evaluation criteria based on AlphaFold3 interface confidence (ipTM) and RMSD self-consistency, we find that Germinal was the only method to generate designs passing stringent in silico criteria for experimental testing. We therefore performed a larger Germinal design campaign employing three different VHH frameworks and experimentally validated 46 designs in vitro. Of these, 42 expressed as soluble proteins and we identified four binding hits derived from two of the three tested frameworks. Of the four binders, two lead candidates were further characterized and demonstrated high affinity (KDs of 4.1 nM and 10.8 nM), monomeric behavior and low polyreactivity, indicating favorable biophysical and developability properties, as well as functional toxin neutralization in vitro. To assess their therapeutic potential we investigated their ability to protect against -cobratoxin toxicity in vivo. Both candidates fully protected mice after -cobratoxin challenge, with 100% survival compared to a lethal control. One candidate also retained notable neutralization capacity against whole venom of Naja kaouthia with a survival of 56%, while the other protected 22% when tested in a rescue setting. Together, we demonstrate that de novo VHH design can generate high affinity single-domain antibodies with in vivo protection against lethal cobra venom neurotoxicity, and provide practical insights into method- and framework-dependent performance.

bioengineering↗

Simple Feedback for Complex Movement: Capturing Whole-Limb Reorganization during Single-IMU Gait Retraining

Clinical gait retraining typically relies on multi-sensor arrays and high-dimensional feedback displays, imposing setup and interpretation burdens that limit routine clinical deployment. We developed a single-IMU visual biofeedback system that delivers real-time feedback of Lower Limb Trajectory Error (LLTE), a composite kinematic error metric integrating knee position and shank angle across the stance phase. Twenty able-bodied adults walked on a treadmill under two visual biofeedback targets (flexed-knee, extended-knee) while receiving either corrected (n=10) or uncorrected (n=8) feedback, where the correction accounted for limb orientation at initial contact. LLTE and stance-phase knee kinematics adapted consistently under the flexed-knee target for both feedback groups, with feedback formulation moderating the temporal trajectory of change. Adaptation toward the extended-knee target was limited, likely because participants were already operating near terminal knee extension and because the scalar error metric provided limited directional information for correction. Ankle range of motion (ROM) changed significantly across the stance phase under both target conditions, while hip ROM did not. Multiscale multivariate sample entropy (MSMVSE) increased monotonically with time scale across all conditions, with no statistically distinguishable difference between corrected and uncorrected feedback. These results suggest that single-IMU LLTE biofeedback can modify gait mechanics and that adaptation was expressed across multiple lower-limb segments rather than through changes at a single joint.

bioengineering↗